Density worked. Took some measurements, did some weighing .. all my materials came out to the expected products within about 1% error.

Lots of UHMW as expected, some PTFE, and couple of 1/2" thick 4" wide, 18" long sheets of Delrin, and one nice 12" x 6" x 1/2" sheet of Ketron Peek. Surprised, about $1000 worth of exotic plastics (at McMaster prices) .... most of that stuff came from people that donated it cause they know I make a lot of projects, or scrap that I picked up at auctions.

Already laminated the density chart to go in my shop info binder

Shame the Delrin is in 1/2" sheets, would be a pain to machine into bushing.

__________________
I'm World's Best Hyperbolist !!
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:47 AM.

 

About Us

The PY Online Forums is the largest online gathering of Pontiac enthusiasts anywhere in the world. Founded in 1991, it was also the first online forum for people to gather and talk about their Pontiacs. Since then, it has become the mecca of Pontiac technical data and knowledge that no other place can surpass.

 




Copyright © 2017