View Single Post
  #14  
Old 06-20-2021, 09:39 AM
MUSLCAH MUSLCAH is offline
Ultimate Warrior
 
Join Date: Sep 2015
Location: N.H.
Posts: 1,923
Default

Quote:
Originally Posted by funkybird View Post
Muslcah I like that fibreglass idea.

are you putting the fibreglass matting on dry, or dipping it in fibreglass resin and then layering on top of the filler?

I guess when it dries the filler does the same job as the resin?
Not using resin …..I take the pre cut fiberglass cloth and smear the SEM bumper bite into the cloth ,on both sides and apply as many layers to fill MOST of the void. Make sure you put a coat of bumper bite on the bumper area …before you apply the first piece of cloth….like laying down bathroom tile